DTA – Differential Thermal Analysis – & DSC – differential scanning calorimetry – measure, respectively, the temperature difference and the heat flow difference between a sample and a reference material (subjected to the same temperature variation in a controlled atmosphere).

DTA detects any change in all categories of materials; DSC determines the temperature and heat of transformation.